論文・報道

2016

No. Pub.,
Book
or
Other
Title Authors Journal Volume Page Year
No. Pub.,
Book
or
Other
Title Authors Journal Volume Page Year
2016_01 Pub. Complex hydride for composite
negative electrode-applicable
to bulk-type all-solid-state
Li-ion battery with wide
temperarture operation
K. Yoshida
S. Suzuki
J. Kawaji
A. Unemoto
S. Orimo
Solid State Ionics 285 96-100 2016
2016_02 Pub. Fast lithium-ionic conduction in a new complex hydride-sulphide crystalline phase A. Unemoto
H. Wu
T.J. Udovic
M. Matsuo
T. Ikeshoji
S. Orimo
Chemical Communications 52 564-566 2016
2016_03 Pub. Liquid-like ionic conduction in solid lithium and sodium monocarba-closo-decaborates near or at room temperature W.S. Tang
M. Matsuo
H. Wu
V. Stabile
W. Zhou
A.A. Talin
A.V. Soloninin
R.V. Skoryunov
O.A. Babanova
A.V. Skripov
A. Unemoto
S. Orimo
T.J. Udovic
Advanced Energy Materials 6 1502237
(1-6)
2016
2016_04 Pub. Stabilizing lithium and sodium fast-ion conduction in solid polyhedral-borate salts at device-relevant temperatures W.S. Tang
M. Matsuo
H. Wu
V. Stavila
A. Unemoto
S. Orimo
T.J. Udovic
Energy Storage Materials 4 79-83 2016
2016_05 Pub. Metallic intermediate Hhdride phase of LaMg2Ni with Ni-H covalent bonding: Precursor state for complex hydride formation K. Miwa
T. Sato
M. Matsuo
K. Ikeda
T. Otomo
S. Deledda
B.C. Hauback
G. Li
S. Takagi
S. Orimo
The Journal of Physical Chemistry C 120 5926-
5931
2016
2016_06 Pub. Extending the applicability of the goldschmidt tolerance factor to arbitrary ionic compounds
(Open Access)
T. Sato
S. Takagi
S. Deledda
B.C. Hauback
S. Orimo
Scientific Reports 6 23592
(1-10)
2016
2016_7 Pub. Corrigendum to recent progress in hydrogen-rich materials from the perspective of bonding flexibility of hydrogen (vol 109, pg 1, 2015) S. Takagi
S. Orimo
Scripta Materialia 116 157 2016
2016_08 Other 新規イオン伝導体群としての錯体水素化物-材料探索と全固体電池への実装- 松尾元彰
宇根本篤
折茂慎一
Electrochemistry 84 26-30 2016
2016_09 Other J-PARCで見えたもの ー大強度パルス中性子源の威力 瀬戸秀紀
高木成幸
海野昌喜
森一広
月刊化学 71 70-71 2016
2016_10 Pub. Complex and liquid hydrides for energy storage
(Invited Paper)
E. Callini
Z.Ö.K. Atakli
B.C. Hauback
S. Orimo
C. Jensen
M. Dornheim
D. Grant
Y.W. Cho
P. Chen
B. Hjorvarsson
P. de Jongh
C. Weidenthaler
M. Baricco
M. Paskevicius
T.R. Jensen
M.E. Bowden
T.S. Autrey
A. Zütte
Applied Physics A 122 353
(1-22)
2016
2016_11 Pub. Complex hydrides as room-temperature solid electrolytes for rechargeable batteries
(Invited Paper, Open Access)
P.E. de Jongh
D. Blanchard
M. Matsuo
T.J. Udovic
S. Orimo
Applied Physics A 122 251
(1-6)
2016
2016_12 Pub. Effect of the structural evolution on the ionic conductivity of Li-N-H system during the dehydrogenation B. Paik
M. Matsuo
T. Sato
L. Qu
A.R. Wolczyk
S. Orimo
Applied Physics Letters 108 213903
(1-5)
2016
2016_13 Pub. 錯体水素化物固体電解質と硫化物ガラス固体電解質の ハイブリッド利用による室温動作可能な4 V 級バルク型 全固体リチウム二次電池の開発 宇根本篤
野上玄器
田沢勝
谷口貢
折茂慎一
日本金属学会誌 80 720-725 2016
2016_14 Pub. 新規金属水素化物の高温高圧合成 齋藤寛之
高木成幸
折茂慎一
青木勝敏
粉体および
粉末冶金
63 298-305 2016
2016_15 Pub. Impact of severe plastic deformation on microstructure and hydrogen storage of titanium-iron-manganese intermetallics K. Edalati
M. Matsuo
H. Emami
S. Itano
A. Alhamidi
A. Staykov
D.J. Smith
S. Orimo
E. Akiba
Z. Horita
Scripta Materialia 124 108–111 2016
2016_16 Pub. Bulk-type all-solid-state lithium batteries using complex hydrides containing cluster-anions A. Unemoto
K. Yoshida
T. Ikeshoji
S. Orimo
Materials Transactions 57 1639-
1644
2016
2016_17 Pub. Hydrogen release reactions of Al-based complex hydrides enhanced by vibrational dynamics and valences of metal cations T. Sato
A.J.
Ramirez-Cuesta
L. Daemen
Y.–Q. Cheng
K. Tomiyasu
S. Takagi
S. Orimo
Chemical Communications 52 11807-
11810
2016
2016_18 Pub. Stabilizing superionic-conducting structures via mixed-anion solid solutions of monocarba-closo-borate salts W.S. Tang
K. Yoshida
A.V. Soloninin
R.V. Skoryunov
O.A. Babanova
A.V. Skripov
M. Dimitrievska
V. Stavila
S. Orimo
T.J. Udovic
ACS Energy Letters 1 659-664 2016
2016_19 Pub. Carbon-rich active materials with macrocyclic nanochannels for high-capacity negative electrodes in all-solid-state lithium rechargeable batteries S. Sato
A. Unemoto
T. Ikeda
S. Orimo
H. Isobe
Small 12 3381-
3387
2016

<< 戻る